Master Bond One Component Epoxy Supreme 10HTF
Subcategory: Epoxy; Thermoset; Polymer
Material Notes: “Snap cure” version of Supreme 10HT with similar physical and electrical properties. Cures in 2 minutes at 375°F. Also available in nickel and silver filled versions.Information provided by Master Bond Inc.
| Available Properties |
- Viscosity
- Storage Temperature
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
|
|
|
|