Master Bond UV Curable Adhesive UV14-3
Subcategory: Thermoset; Polymer
Material Notes: Flexible adhesive, sealant and encapsulant. Easily removable by conventional solvents. Has a low index of refraction (1.477).Information provided by Master Bond Inc.
| Available Properties |
- Viscosity
- Hardness, Shore D
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|