Master Bond Anaerobic Adhesive GP222
Subcategory: Thermoset; Polymer
Material Notes: “no drip”; for quick disassembly; for locking, bonding and sealing.Strengths and cure time measured with unprimed clean 3/8-24 carbon steel fasteners. Strengths reported after 24 hour cure at room temperature in accordance with MIL-S-22473D Information provided by Master Bond Inc.
| Available Properties |
- Viscosity
- Impact Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
- Typical Gap Filled, inches
|
|
|
|
| Property Data |