Master Bond Mastersil Two Component Silicone Adhesive 150
Subcategory: Silicone; Thermoset; Polymer
Material Notes: Non-corrosive, condensation type cure. For electronic potting & encapsulation. High flexibility & low shrinkage upon cure.Information provided by Master Bond Inc.
| Available Properties |
- Viscosity
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Yield
- Volume Resistivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color Code
- Mix Ratio by weight
- Set-Up Time, minutes
|
|
|
|
| Property Data |