Master Bond Mastersil One Component Silicone Adhesive 726
Subcategory: Silicone; Thermoset; Polymer
Material Notes: Thermally conductive grease (conductivity of 5-6 BTU•in/ft2 •hr•°F at 75°F). Meets MIL C47113A. Information provided by Master Bond Inc.
| Available Properties |
- Volume Resistivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
- Viscosity
|
|
|
|