Master Bond Polymer System EP30D-14
Subcategory: Epoxy; Thermoset; Polymer
Material Notes: Two Component, Optically Clear Room Temperature Curing Urethane Elastomer System Featuring Superior Strength, Toughness, and Chemical Resistance For High Performance Bonding, Sealing, Potting And Encapsulation ApplicationsMaster Bond Polymer System EP30D-14 is a uniquely versatile two component optically clear urethane elastomer featuring superior strength, toughness and chemical resistance for high performance bonding, sealing, casting, potting and encapsulation applications. It combines the recognized advantageous performance characteristics of epoxy resins such as strength, chemical resistance and adhesive qualities, with those of the polyurethanes characteristic toughness, abrasion resistance and toughness. Master Bond Polymer System EP30D-14 is formulated to cure at room temperature or more rapidly at elevated temperatures, with a user friendly one to one noncritical mix ratio on a weight basis. It is 100% reactive and does not contain any solvents or diluents. This specially clear, low viscosity polymer system cures with minimal shrinkage to a remarkably high strength and tough thermoset plastic with very superior resistance to thermal cycling and chemicals including water, inorganic salts, alkalis and acids. Adhesion to metals, glass, concrete, ceramics, wood, vulcanized rubbers and many plastics is excellent. The cured material is an electrical insulator. Color of part A is clear, part B clear. Master Bond Polymer System EP30D-14 is widely used in the electronic, electrical, computer, construction, metalworking, appliance, automotive and chemical process industries. It is quite safe to use when proper industrial hygiene practices are observed viscosities and cure times can be readily adjusted within wide limits so as to best meet specific application requirements. Information provided by Master Bond Inc.
| Available Properties |
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color Code
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|