Master Bond Polymer System X-5TC

 

Subcategory: Epoxy; Thermoset; Polymer

Material Notes:
Thermally Conductive, Elastomer Based, One-Component Adhesive For High Performance Bonding and Sealing

Master Bond X-5TC is an aluminum oxide filled, thermally conductive elastomer-based, one component adhesive for high performance bonding and sealing. This thermally conductive adhesive bonds well in both shear and peel to similar and dissimilar surfaces including metals, woods, most plastics, ceramics, glass, rubber, paper, leather, wallboard and insulation, concrete, plastic foams and stone. Master Bond X-5TC contains a small amount (6%) of a ketone solvent which evaporates as cure proceeds. An initial set takes place in Master Bond X-5TC as soon as most of the solvent has evaporated. The strength of this initial set usually suffices to maintain the assembly and, with some adherends, will exceed the strength of the material. Bond strength increases as evaporation of the solvent progresses, reaching a maximum when all of the solvent has been removed. All surfaces should be carefully cleaned and dried before application. They should be free of grease, oil, dirt and other contaminants for optimal results. Conventional cleaning methods such as solvent washing, vapor degreasing, etching, etc. are applicable. A convenient way of determining when through cleaning has been accomplished is to flow water over a vertically held coated surface. If the water runs off in a continuous film, cleaning is satisfactory. Master Bond X-5TC is an easily flowable paste. It can be thinned with ketone solvents to reduce viscosity.

Information provided by Master Bond Inc.

Available Properties
  • Solids Content
  • Surface Resistivity per Square
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。