Master Bond Polymer System LTX 123
Subcategory: Epoxy; Thermoset; Polymer
Material Notes: Water-Borne Aliphatic Urethane For High Performance Adhesives and CoatingsMaster Bond Polymer System LTX123 is a light stable aliphatic urethane composition with excellent adhesive properties particularly to vinyl, polyester, polyethylene and nylon substrates. Adhesive to glass is likewise very good. Master Bond Polymer System LTX123 offers an outstanding combination of heat resistance, gloss and slip, non-yellowing behavior and excellent solvent resistant. This product should be stored in closed containers and kept from freezing. Information provided by Master Bond Inc.