The Matrixx Group 12N7006 Flame Retardant (V2) Copolymer Polypropylene (High Flow, High Impact)
Subcategory: Polypropylene; Thermoplastic
Material Notes: Data provided by The Matrixx Group, formerly RePlas.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Gardner Impact @ 23°C
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Flammability, UL94
|
|
|
|