Ellay Ellay™ PVC 0-4115 Plasticized Polyvinyl Chloride Biomedical Elastomer
Subcategory: Vinyl; Elastomer, TPE; Thermoplastic
Close Analogs: Ellay, Inc. was acquired by the Solvay Group in 1999.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
|
|
|
|