Meilian Chemical Co. WHITE MASTERBATCH PE12077
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: WHITE PE12077 is a LDPE based masterbatch containing high-quality TiO2 without any addition of filler or fluorescence whitener. It is designed for use in economy films for general purpose, especially in shopping bags and geomembrane.Method of Usage: WHITE PE12077 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, free from pollution problem caused by pigment. Range of Application: WHITE PE12077 is designed for LDPE, HDPE, LLDPE, and PP.