Meilian Chemical Co. BLACK MASTERBATCH PE2306
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: BLACK PE2306 is an economy black low density polyethylene based masterbatch containing high opacity carbon black. This product is designed for general-purpose films with high tinting strength, especially for use in HDPE.Method of Usage: BLACK PE2306 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resin in mixer, avoiding pollution and malscattering problems caused by pigment. Range of Application: BLACK PE2306 is designed for use in LDPE, HDPE, LLDPE, and PP.
| Available Properties |
- Density
- Melt Index of Compound
- Carrier
- Compatibility
- Pigment Content: Carbon Black (%)
|
|
|
|