Meilian Chemical Co. GREEN MASTERBATCH PE650
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: GREEN PE650 is a green LDPE based masterbatch containing 30% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Green 7.Method of Usage: GREEN PE 650 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, avoiding pollution and malscattering problems caused by pigment. Range of Application: GREEN PE650 is designed for use in LDPE, HDPE, LLDPE and PP for production of premium high glossy films.
| Available Properties |
- Density
- Melt Index of Compound
- Carrier
- Compatibility
- Pigment Content
|
|
|
|