Meilian Chemical Co. BLUE MASTERBATCH PE82172
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: BLUE PE82172 is a blue LDPE-based masterbatch containing 30% Phthalocyanine Pigment. It is designed for outdoor products with excellent dyeing strength and weathering resistance. Color Index No.:Blue 15:3Method of Usage: BLUE PE82172 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, without the necessity of prior drying. Range of Application: BLUE PE82172 is designed for use in LDPE, HDPE, LLDPE and PP for production of films, sheets, plates, hollowing blow molding and direct injection molding in shaper.
| Available Properties |
- Density
- Melt Index of Compound
- Carrier
- Compatibility
- Pigment Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|