Meilian Chemical Co. RED MASTERBATCH PE305A
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: RED PE 305A is a red LDPE-based masterbatch containing 32% pigment, designed for use in polyolefin resins (PE and PP, etc..). Color Index No.: Red 53:1Method of Usage: RED PE 305A is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, avoiding pollution and malscattering problems caused by pigment. Range of Application: RED PE 305A is designed for use in LDPE, HDPE, LLDPE and PP for premium high gloss films with excellent gloss levels and optimum printability.
| Available Properties |
- Density
- Melt Index of Compound
- Carrier
- Compatibility
- Pigment Content
|
|
|
|