Meilian Chemical Co. RED MASTERBATCH PE62071
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: RED 62071 is a red LDPE-based masterbatch containing 30% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Red 48:1.Method of Usage: RED PE62071 is designated for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, avoiding pollution and malscattering problems caused by pigments. Range of Application: RED PE 62071 is designed for use in LDPE, HDPE, LLDPE and PP for production of premium high glossy film, sheet and plate, and for applications of Hollow Blown Molding and sharper direct Injection Molding.
| Available Properties |
- Density
- Melt Index of Compound
- Carrier
- Compatibility
- Pigment Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|