Orbis Static Intercept (SI) Polypropylene Copolymer Resin
Subcategory: Polypropylene; Thermoplastic
Material Notes: High impact, injection molded resin. Permanently static dissipative. Containers made with this material are unaffected by humidity and do not outgas harmful contaminants. Test results show injection molded totes contain no detectable signs of silicon, amides, chlorides, hydrocarbons, or esters, making them cleanroom safe. Orbis makes containers from this resin. Data provided by Orbis, Menasha Corporation.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Electrical Resistivity
- Surface Resistance
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,