Merquinsa Pearlthane® D11T60 Thermoplastic Polyurethane
Subcategory: Polyurethane, TP; Thermoplastic
Key Words: TPU
Material Notes: Polyester-based TPU, supplied in form of translucent, colorless or slightly yellowish pellets, combining very high hardness with excellent mechanical properties. It is especially advisible for use in producing technical parts by injection molding. Apllications: Shoe heels, Top pieces, Rollers, Ear-tags, injection-molded components Information provided by Merquinsa
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Tear Strength
- Abrasion
- Compression Set
- Compression Set, Elevated Temperature
- Melting Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|