Merquinsa Pearlthane® D11T70 Polycaprolactone Copolyester based TPU

 

Subcategory: Polyurethane, TP; Thermoplastic

Material Notes:
Pearlthane® 11 series is based on Merquinsa`s proprietary polycaprolactone (PCL) technology. It offers a unique combination of key benefits vs. standard TPU polyesters:

  • Significant lower part cost because of intrinsic lower density and faster processing
  • Superior performance such as hydrolysis resistance, abrasion resistance and low temperature impact properties.

Plasticizer-free soft polycaprolactone grade designed for TPE compounds and soft touch ergonomic applications. It can be extruded and injection moulded.

Applications: Injection moulding: Automotive parts, and overmoulding.
Extrusion and compounding: Wire bound hoses, TPE compounding, belts & profiles such as timing belts, hose sheathing, and pneumatic tubing, elastic/barrier films, and compounding.

The values shown are typical values and should not be used for establishing specifications.

Available Properties
  • Density
  • Melt Index of Compound
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 100% Modulus
  • 300% Modulus
  • Tear Strength
  • Abrasion
  • Compression Set
  • Transformation Temperature, Tg
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。