Merquinsa Pearlthane® 11T65D Polycaprolactone Copolyester based TPU
Subcategory: Polyurethane, TP; Thermoplastic
Material Notes: Pearlthane® 11 series is based on Merquinsa`s proprietary polycaprolactone (PCL) technology. It offers a unique combination of key benefits vs. standard TPU polyesters:- Significant lower part cost because of intrinsic lower density and faster processing
- Superior performance such as hydrolysis resistance, abrasion resistance and low temperature impact properties.
Fast cycling and abrasion resistance for injection moulding applications. Applications: Automotive parts such as wheels, shoe heels, overmoulding, and other technical parts. The values shown are typical values and should not be used for establishing specifications.
| Available Properties |
- Density
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Abrasion
- Compression Set
- Transformation Temperature, Tg
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|