Merquinsa Pearlthane® 15N80 Polyether Polycaprolactone Copolymer based TPU
Subcategory: Polyurethane, TP; Thermoplastic
Material Notes: This special polyether polycaprolactone copolymer product range is tailor-made to meet a wide range of specific needs such as high heat resistance and elasticity in blown film applications or outstanding mechanical properties for long term animal identification tags.Injection moulding and extrusion copolymer grade offering excellent processing behavior. Main properties are elasticity, high hydrolysis resistance, transparency and good mechanical properties, as well as wear resistance. Widely used for elastic films or injected for technical parts. Applications: Injection moulding: Automotive parts, gasket & seals, mining screens, snow parts, goggles, and overmoulding Extrusion and compounding: Elastic film weather resistant, high heat film performance. Extrusion and compounding: Elastic/barrier films, belts & profiles, transparent tubing, and wire bound hoses. The values shown are typical values and should not be used for establishing specifications.
| Available Properties |
- Density
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Abrasion
- Compression Set
- Transformation Temperature, Tg
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|