Merquinsa Pearlthane® D16N95 Polyether based TPU

 

Subcategory: Polyurethane, TP; Thermoplastic

Material Notes:
Pearlthane® and Pearlcoat® grades of this series are used when superior hydrolysis resistance, outstanding low temperature flexibility or good microbiological protection is required. This polyether range is typically used for marine applications, geophysical cables and winter sport applications.

Extrusion grade with very good mechanical properties and processability. Ideal for outdoor applications. Suitable for specific injection moulding applications.

Applications: Injection moulding: Automotive parts, gasket & seals, mining screens, snow parts, goggles, and overmoulding.
Extrusion and compounding: Cables, fire hoses, and breathable HMVT.
Extrusion and compounding: Elastic/barrier films, belts & profiles, pneumatic tubing, transparent tubing, and outdoor cables.
Melt Coating: Inflatable items.

The values shown are typical values and should not be used for establishing specifications.

Available Properties
  • Density
  • Melt Index of Compound
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 100% Modulus
  • 300% Modulus
  • Tear Strength
  • Abrasion
  • Compression Set
  • Transformation Temperature, Tg
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。