Merquinsa Pearlthane® D16N85UV Polyether based TPU
Subcategory: Polyurethane, TP; Thermoplastic
Material Notes: Pearlthane® and Pearlcoat® grades of this series are used when superior hydrolysis resistance, outstanding low temperature flexibility or good microbiological protection is required. This polyether range is typically used for marine applications, geophysical cables and winter sport applications.Wire and cables, hoses and film extrusion grade exhibiting low gels, low temperature flexibility, excellent hydrolysis and microbe resistance. D16N85UV is the UV version of this grade. Suitable also for specific injection moulding applications. Applications: Extrusion and compounding: Fire hoses, and breathable HMVT, elastic/barrier films, belts & profiles, transparent tubing, outdoor cables, and wire bound hoses. Melt Coating: Inflatable items. The values shown are typical values and should not be used for establishing specifications.
| Available Properties |
- Density
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Abrasion
- Transformation Temperature, Tg
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|