Merquinsa PEARLBOND® 106 Linear Thermoplastic Polyurethane
Subcategory: Polyurethane, TP; Thermoplastic
Material Notes: PEARLBOND® 106 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a very high thermoplasticity level.Applications: PEARLBOND® 106 is mainly used for making heat-sealable fabrics (Thermobonding), obtained by coating processes such as scattering or dot-coating (powder or paste). In all cases, the product is previously ground into powder, by cryogenic grinding. The particle size of the powder will depend on the application technique to be used.
| Available Properties |
- Density
- Viscosity
- Brookfield Viscosity
- Melt Flow
- Hardness, Shore A
- Melting Point
- Softening Point
- Crystallization rate (minutes)
- Thermoplasticity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|