Merquinsa PEARLBOND® 151 Linear Thermoplastic Polyurethane
Subcategory: Polyurethane, TP; Thermoplastic
Material Notes: PEARLBOND® 125/H is polycaprolactone-based thermoplastic polyurethane, supplied in form of colourless or slightly yellowish, translucid pellets, combining a low hardness with excellent low-temperature flexibility.Applications: PEARLBOND® 151 is used for textile coating for making shoe-stiffeners (toe puffs & counters), by extrusion or sintering process.
| Available Properties |
- Density
- Brookfield Viscosity
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Melting Point
- Softening Point
|
|
|
|