Merquinsa PEARLBOND® 521 Linear Thermoplastic Polyurethane
Subcategory: Polyurethane, TP; Thermoplastic
Material Notes: PEARLBOND® 521 is a linear, polycaprolactone-copolyester polyurethane with a very high crystallization rate and a very high thermoplasticity level.Applications: PEARLBOND® 521 can be added to formulations of REACTIVE POLYURETHANE HOT-MELTS, in order to improve the crystallisation speed.
| Available Properties |
- Density
- Viscosity
- Melt Flow
- Total Base Number
- Melting Point
- Moisture Content
- Crystallization rate (minutes)
- Thermoplasticity
|
|
|
|