M. Holland CP410 Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Discontinued Grade
Material Notes: Features: Copolymer, Low Temp. Medium Impact Resistance Uses: Automotive Interior Parts, Furniture, Sporting Goods, Tool/Tote Box Processing Method: Injection Molding Information provided by M. Holland.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Form
|
|
|
|