M. Holland CP800 Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Discontinued Grade
Material Notes: Additives: Nucleating Agents Features: Fast Cycle (Production), High Flow, Good Impact Resistance, Nucleated, Good Stiffness Uses: Containers, Household Goods, Thin-walled Parts Processing Method: Injection Molding Information provided by M. Holland.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Gardner Impact
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|