M. Holland GS411 Polystyrene
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Discontinued Grade
Material Notes: Features: Good Crack Resistance, Crystal, Fast Cycle (Production), Good Flow Uses: Disposable Drinkware, Electrical/Electronic Applications Approvals: FDA 21 CFR 177.1640 Processing Method: Extrusion, Injection Molding Information provided by M. Holland.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Form
|
|
|
|