M. Holland IS350 Polystyrene, High Impact
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Discontinued Grade
Material Notes: Uses: Audio Tapes, Structural Foam, Household Goods, Housings, Toys Processing Method: Injection Molding Information provided by M. Holland.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Flexural Modulus
- Izod Impact, Notched
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|