M. Holland LL217AA LLDPE
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Close Analogs: Discontinued Grade
Material Notes: Features: High Clarity, Copolymer, Good Processability Uses: Film, Cast Film Approvals: FDA 21 CFR 177.1521 Processing Method: Blown Film and Cast Film Information provided by M. Holland.
| Available Properties |
- Density
- Melt Flow
- Secant Modulus, MD
- Secant Modulus, TD
- Dart Drop Test
- Haze
- Form
|
|
|
|