M. Holland PC500-1 Polycarbonate
Subcategory: Polycarbonate; Thermoplastic
Close Analogs: Discontinued Grade
Material Notes: Additives: UV Stabilizer Features: High Flow, Good Impact Resistance, Good UV Resistance Uses: Safety Guards, Telecommunications Processing Method: Injection Molding Information provided by M. Holland.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Appearance
- Form
|
|
|
|