M. Holland PP202 Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Discontinued Grade
Material Notes: Features: Homopolymer, Low Residuals, Good Stiffness, High Viscosity Approvals: FDA 21 CFR 177.1520 Information provided by M. Holland.