M.Holland PS (GPPS) GS230 Polystyrene, General Purpose
Subcategory: Polystyrene; Thermoplastic
Material Notes:
- High heat resistance
- Good processability
- High strength
Applications: - Bottles
- Business equipment
- Medical applications
- Packaging
| Available Properties |
- Melt Flow
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Forms
- Processing Methods
|
|
|
|