Micropol Microcene MC122 Metallocene Based Polyethylene Rotational Molding Powder
Subcategory: Polyethylene; Thermoplastic
Material Notes:
Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. Information provided by Micropol Limited
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |