Micropol Microcoat DG/EVA/214A Microground modified EVA copolymer
Subcategory: Ethylene Vinyl Acetate
Material Notes: Specially developed for high specification coating where metal/coating adhesion is of primary importance. Typically used on large flat surfaces, and when toughness, elasticity and excellent barrier properties are needed. Information provided by Micropol Limited
| Available Properties |
- Specific Gravity
- Particle Size
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |