Mid-Mountain Materials Hytex® 700 Kevlar® Glass Industrial Textile
Subcategory: Aramid; Composite Fibers
Key Words: poly-paraphenylene terephthalamide, poly p-phenylene, aramid fiber, FRP composites
Material Notes: Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemistry and in differing configurations (cloth, tape, sleeving, rope etc.). Mid-Mountain can design hybrid materials by blending most any combination of yarns. HYTEX® 700 textile products are produced from blended yarns of Kevlar® and glass fibers. The blend combines the wear resistance of fiberglass with the tensile strength of Kevlar® to produce products with good strength and abrasion resistance at temperatures to 650ºF • 345ºC. Strength and dimensional stability are excellent while weight is low. HYTEX® 700 textiles are especially suited for use in heat shields, curtains, and various insulating applications. Information provided by Mid-Mountain Materials.
| Available Properties |
- Maximum Service Temperature, Air
- Decomposition Temperature
- Abrasion Resistance
- Acid Resistance
- Alkali Resistance
- Color
- Composition
- Solvent Resistance
- Sunlight & Aging Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|