Mikro-Technik Reproflon G25 PTFE
Subcategory: Fluoropolymer; Thermoplastic; PTFE; Polymer
Material Notes: Available Forms: Rods, Tubes. Special Characteristics: Higher resistance to abrasionHigher resistance to compression compared to virgin PTFE and unfilled ReproflonReduced plastic flowInformation provided by Mikro-Technik GmbH