Mikro-Technik Carboxymethylcellulose (CMC) DT R

 

Subcategory: Cellulosic

Material Notes:
Purified Grade

Comments:

  • All grades are available neutralized with carbon dioxide (no suffix or suffix K) or acetic acid (suffix E).
  • Reduced active contents down to 50 % are available. Special concentrations on request.
  • Most of the grades are available as powder or granules. Special granulometry on request.
  • The viscosity ranges listed above are typical. Narrower ranges and special viscosities are available on request.

    Information provided by Mikro-Technik GmbH

    Available Properties
    • Viscosity
    • Degree of Substitution
    • Max. Active Content %, on dry basis
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
  • 请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。