PolyMirae Moplen EP340K Sheet and Thermoforming Grade Polypropylene
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: Moplen RP340K is the polypropylene random copolymer polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340K is a random copolymer particularly suitable for sheet for stationary & packaging. Moplen RP340K resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Excellent clarity; Excellent gloss and surface appearance; Good processability; Low blooming in use; Good melt tension Applications: Transparent sheet for stationary and packaging Information provided by PolyMirae Company Ltd.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|