PolyMirae Moplen EP400M Injection Molding Grade Polypropylene
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: Moplen EP400M is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP400M is a block copolymer particularly suitable for injection molding of parts of electrical appliances, containers, battery case. Moplen EP400M meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520. And the components of additives are adequate on the food packaging substances specification of FDA regulation 21 CFR 178.2010. Features: Optimized balance of stiffness and toughness; High Impact strength at low temperature; High stiffness; Low warpage Applications: Parts of electrical appliances; Containers; Battery case Information provided by PolyMirae Company Ltd.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|