PolyMirae Moplen EP648N Injection Molding Grade Polypropylene
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: Moplen EP648N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP648N is a high gloss block copolymer particularly suitable for injection molding of parts of electrical appliances, containers. Moplen EP648N meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520. Features: Optimized balance of stiffness and toughness; High gloss; High stiffness; Heat resistance; Scratch resistance; Applications: Parts of electrical appliances; Containers Information provided by PolyMirae Company Ltd.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|