PolyMirae Moplen HP500G Sheet and Thermoforming Grade Polypropylene
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: Moplen HP500G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP500G is a homopolymer particularly suitable for sheet, thermoforming and stripe. Moplen HP500G resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Excellent processibility and stretchability; High mechanical properties; High melt strength Applications: Food packaging and tray (Thermoforming); Bottle (Blow molding); Blown film; High strength for rope, container bag, extruded nets Information provided by PolyMirae Company Ltd.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|