PolyMirae Moplen HP563S Fiber (Spunbond) Grade Polypropylene
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: Moplen HP563S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP563S is a homopolymer particularly suitable for spunbonded nonwovens. Moplen HP563S resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Excellent spinnability; Excellent drawability; Odorless; Narrow molecular weight distribution; Anti-gas fading Applications: Diaper and Sanitary Napkin; Agriculture; Shopping Bag; Apparel Cover; Wet Tissues Information provided by PolyMirae Company Ltd.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|