Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
Subcategory: Nylon; Thermoplastic; Polymer
Material Notes: ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses strong dimensional stability and chemical resistance. In addition, the effect of water absorption, which is a traditional weakness of polyamides, has been reduced to a minimum. Applications: - Cylinder head covers
- Thermostat cases
- Oil pump housings
- Hydraulic system pistons
- Cooling system parts
- Roller/pulley parts
Information provided by Mitsui.
| Available Properties |
- Density
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Feed Temperature
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Mold Temperature
- Screw Speed
- Injection Pressure
- Injection Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|