Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
Subcategory: Polyimide; Thermoplastic
Material Notes: AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to its semicrystalline state. In addition, it displays low outgassing, superior radiation resistance and excellent chemical resistance properties. Applications: - Components for automotive and aircraft engines
- Transmission
- Farming, off-road and construction equipment
- Industrial machinery
- Electric motors, pumps and compressors
- Business machines such as laser pointers and high speed copy machines
- Electronic and semiconductor transport media
- Analytical and medical equipment
- Conveyors and textile equipment
Information provided by Mitsui.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Hardness, Rockwell M
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Ultimate at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Compressive Modulus
- Shear Strength
- Izod Impact, Notched
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Glass Temperature
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|