Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous

 

Subcategory: Polyimide; Thermoplastic

Material Notes:
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to its semicrystalline state. In addition, it displays low outgassing, superior radiation resistance and excellent chemical resistance properties.

Applications:

  • Components for automotive and aircraft engines
  • Transmission
  • Farming, off-road and construction equipment
  • Industrial machinery
  • Electric motors, pumps and compressors
  • Business machines such as laser pointers and high speed copy machines
  • Electronic and semiconductor transport media
  • Analytical and medical equipment
  • Conveyors and textile equipment

Information provided by Mitsui.

Available Properties
  • Density
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Linear Mold Shrinkage
  • Tensile Strength at Break
  • Elongation at Break
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • CTE, linear 20°C
  • CTE, linear 20°C Transverse to Flow
  • Thermal Conductivity
  • Melting Point
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。