Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled

 

Subcategory: Polyimide; Thermoplastic; Polymer

Material Notes:
AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber reinforced AURUM JGN3030 offers a unique balance of mechanical and thermal properties for superior performance in demanding automotive, business machinery, industrial equipment, aerospace, and semiconductor equipment applications. AURUM exhibits outstanding resistance to chemicals and radiation, a low coefficient of thermal expansion, excellent electrical properties, and flame resistance.

Applications: AURUM JGN3030 injection molded components are excellent replacements for metals, ceramics, and other plastics. High performance AURUM JGN3030 parts include heat-resistant gears, semiconductor manufacturing and handling equipment components, and thermal and electrical insulators.

Information provided by DuPont

Available Properties
  • Specific Gravity
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Linear Mold Shrinkage
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Yield
  • Flexural Modulus
  • Flexural Strength
  • Compressive Strength
  • Izod Impact, Notched
  • Surface Resistance
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear 68°F
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Transformation Temperature, Tg
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。