Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade
Subcategory: Polymethylpentene; Thermoplastic
Material Notes: TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equipment, laboratory ware, small appliances, ovenware, baking cartons, release paper, wire and cable coating, and a number of industrial uses. TPX is manufactured and marketed solely by Mitsui Chemicals, Inc. Applications: - Injection Molded Items:
- Blood test cells
- Medical instruments
- Laboratory ware
- Coffee maker parts
- Cosmetic containers
- Extrusion Molded Items:
- Sight glass (pipes, sheets)
- Baking cartons (food containers)
- Release paper
- Wire and cable coating
- Films
Molding Method: Information provided by Mitsui.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Strength
- Izod Impact, Unnotched (ISO)
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|