Mitsui MILEX™ RN-2830MB Acrylic Rubber Modified Phenolic Resin

 

Subcategory: Phenolic; Thermoset

Material Notes:
The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic material is primarily used as binders in brake pad and clutch facing disc friction materials. The advantage of incorporating the MILEX material into a brake design is that the material provides a non-abrasive, vibratory free surface finish, which is very important in the performance of the brake system. Additionally, its superior performance at elevated temperatures and excellent moldability aids in brake noise reduction.

The RN series are novolak type phenolic resins modified by special elastomers. This series consists of a grouping of acrylic rubber modified resin in addition to the RS-2210MB grade, a silicon rubber modified resin. This series is recognized worldwide by the automotive industry for its thermal shock and chemical resistant properties. In addition, this particular series possesses anti-brake noise and vibratory qualities in brake pad applications. Some of the most demanding electrical applications choose phenolic resin due to the material's high dielectric strength, superior insulation resistance and high temperature resistance. Typical applications include use as an Epoxy Resin hardener for electronic materials such as encapsulation for I.C., an adhesive with elastomers and to improve the high heat resistance of thermoplastics.

Applications:

  • Automotive friction materials (brake pads, clutch facing discs, etc)
  • Epoxy resin hardener for electronic materials
  • Additive to improve heat resistance of thermoplastics
  • Adhesives, especially with elastomers, to bond to metal

Information provided by Mitsui.

Available Properties
  • Maximum Service Temperature, Air
  • Processing Temperature
  • Cure Time
  • Cracking Resistance
  • Curing Rate
  • Flow
  • Hardness
  • Heat Resistance
  • Kind of Rubber
  • Rubber Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。